NASA remains in an ongoing test mode to determine what’s behind the ablative thermal protective material that chipped away unexpectedly from the Artemis 1 Orion heat shield during its reentry into Earth’s atmosphere back on Dec. 11, 2022.
The Orion spacecraft for the Artemis 1 mission splashed down in the Pacific Ocean after a 25.5-day mission.
During the high-speed, 25,000 miles per hour return from lunar distance, the thermal protection system of Orion’s crew module must endure blistering temperatures to keep crew members safe. Measuring 16.5 feet in diameter, Orion’s heat shield is the largest of its kind developed for missions carrying astronauts.
Root cause
But in a post-flight analysis of the Artemis 1 heat shield, NASA identified more than 100 locations where ablative thermal protective material was liberated during its speedy reentry.
Work to determine the root cause did conclude last summer, said NASA’s Lori Glaze Deputy Associate Administrator (Acting) Exploration Systems Development Mission Directorate.
Speaking Oct. 29 at the Annual Meeting of the Lunar Exploration Analysis Group being held in Houston, Texas, Glaze did not say what root cause was uncovered.
However, Glaze said that additional testing is ongoing before any final determination is made. That testing will conclude by the end of November, then provided to NASA chief, Bill Nelson, for a final decision.
Artemis II
Meanwhile, NASA is moving forward on readying the Artemis 2 hardware to support hurling a four-person crew to sojourn out beyond the moon, then return to Earth.
The Artemis 2 crew is to depart Earth no earlier than September 2025 on a 10-day trek.
In classic “wait a minute” style, a NASA Office of Inspector General (OIG) report was issued in May of this year – “NASA’s Readiness for the Artemis II Crewed Mission to Lunar Orbit” – calling attention to this issue and others before sending off the first human crew toward the moon since 1972 – the Apollo 17 mission.
To ensure the safety of the crewed Artemis 2 mission, the OIG report recommended the Associate Administrator for Exploration Systems Development Mission Directorate to ensure the root cause of Orion heat shield char liberation is well understood prior to launch of the Artemis 2 mission.
The OIG report called for analysis of Orion separation bolts using updated models that account for char loss, design modifications, and operational changes to Orion prior to the Artemis 2 launch.
The report by the NASA OIG also notes that “human spaceflight by its very nature is inherently risky, and the Artemis campaign is no exception. We urge NASA leadership to continue balancing the achievement of its mission objectives and schedule with prioritizing the safety of its astronauts and to take the time needed to avoid any undue risk.”
Avcoat changes
The heat shield features the same ablative material called Avcoat used in Apollo lunar outings and return-to-Earth missions. However, the building process has changed, according to Lockheed Martin that fashioned Orion’s thermal protection system.
“Instead of having workers fill 300,000 honeycomb cells one by one with ablative material, then heat-cure the material and machine it to the proper shape, the team now manufactures Avcoat blocks – just fewer than 200 – that are pre-machined to fit into their positions and bonded in place on the heat shield’s carbon fiber skin,” the aerospace firm’s website explains. That process is a timesaver in putting on the Avcoat – about a quarter of the time.
So here’s the lingering and nagging question: Is it possible that changes in the Avcoat may be needed? If so, that decision would seemingly necessitate de-coupling the heat shield from the Artemis 2 Orion capsule.
Heat shield hiccups
When the heat shield issue first came to light, Space.com contacted the Orion program office at NASA Johnson Space Center for comment regarding the heat shield hiccups.
“During Artemis 1 post-flight inspection, engineers observed variations of Avcoat material across the appearance of Orion’s heat shield. Some areas of expected charred material ablated away differently than computer modeling and ground testing predicted, and there was slightly more liberation of the charred material during re-entry than anticipated,” the program office stated.
“We expect the material to ablate with the 5,000 degrees Fahrenheit the spacecraft encounters on a re-entry through Earth’s atmosphere, and to see charring of the material through a chemical reaction, but we didn’t expect the small pieces that came off, versus being ablated,” the NASA statements adds.
Healthy margin
“We don’t know yet exactly how much was liberated, which is why we’re analyzing the data, but there was a healthy margin remaining of virgin Avcoat, and temperature data inside the cabin remained at expected levels, so if crew were on board they would not have been in danger,” explains the program office statement.
“It’s still too early in our testing and analysis to arrive at any potential recommendations or solutions that address additional char liberation,” NASA responded. “It’s possible the phenomenon may just [be] part of what the heat shield is, and what we would expect as we return from the moon, but we’ll let the data inform us.”
Lastly, the NASA Orion program office stated: “We’ll continue to protect for variations that could happen during re-entry as we want to ensure we have significant margin against the various types of uncertainties that might occur as the spacecraft re-enters the atmosphere. Our teams want the confidence that we have the best heat shield possible to fly humans going forward.”